 MADw ID: 7585

 

No Image available
Specifics:

Scientific Name: Eucalyptus diversicolor F.V. Muell.
Genus: Eucalyptus
Species :diversicolor
Author :F.V. Muell.
Family :Myrtaceae
Common name :karri
Other :
Collector's date :10/21/1927
Synonym :
Region :AUSTRALIA
Country :Australia
State :Western Australia