 MADw ID: 6607

 

No Image available
Specifics:

Scientific Name: Eucalyptus gigantea Hook.f.
Genus: Eucalyptus
Species :gigantea
Author :Hook.f.
Family :Myrtaceae
Common name :mountain ash, gum topped stringybark
Other :
Collector's date :
Synonym :Eucalyptus delegatensis RT Bak.
Region :AUSTRALIA
Country :Australia
State :New South Wales
Location :