 MADw ID: 1073

 

No Image available
Specifics:

Scientific Name: Eucalyptus camaldulensis Dehn.
Genus: Eucalyptus
Species :camaldulensis
Author :Dehn.
Family :Myrtaceae
Common name :red river gum, eucalyptus
Other :Forests Commission of Victoria E41
Collector's date :
Synonym :Eucalyptus rostrata Shclecht
Region :AUSTRALIA
Country :Australia
State :Victoria
Location :