Title: Thermal stability of metal-lignin composites prepared by coprecipitation method

Source: Thermochimica Acta. 690: 178659.

Author(s)Yan, Qiangu ; Boardman, Charles R.; Cai, Zhiyong

Publication Year: 2020  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-1B   FPL-4716-2A

Abstract: In present work, Fe-lignin composites were prepared by chemical coprecipitation of metal salts and kraft lignin; the thermal stability of the Fe-lignin mixture was then investigated at temperatures up to 300 °C using thermogravimetric analysis (TGA) and diferential scanning calorimetry (DSC) at a heating rate of 5 °C min−1 under nitrogen atmosphere. The structural characteristics of Fe-lignin thermal treated under diferent temperatures were identifed by Fourier transform infrared (FTIR) spectrometry. The temperature-programmed thermal decomposition (TPD) of Fe-lignin samples was carried out in a fxed-bed reactor; the gaseous products were analyzed qualitatively and quantitatively by an on-line quantitative gas ana ysis system. The temperature and pressure of the reactor were monitored and recorded during the thermal decomposition process. It was observed, the therma decomposition of Fe- lignin samples is a strong exothermic process, and a signifcant amount of heat is re eased from the reaction, which triggers a thermal runaway situation.

Keywords: Kraft ignin; Fe-lignin composites; thermal stability; Fe content and solvents ;thermal runaway

Publication Review Process: Formally Refereed

File size: 4,096 kb(s)

Date posted: 08/21/2020

This publication is also viewable on Treesearch:  view
RITS Product ID: 98655
Current FPL Scientist associated with this product
Cai, Zhiyong
Supervisory Research Materials Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »