Title: Limiting polysaccharide motion protects wood from decay

Source: Proceedings article

Author(s)Hunt, Christopher; Zelinka, Samuel; Jakes, Joseph

Publication Year: 2020  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4707-1B   FPL-4716-3A

Abstract: It is well known that chemical modifications to improve decay resistance also reduce the equilibrium moisture content (EMC) of wood. The mechanism of this action, however, has been the subject of much debate. Several groups have suggested that decay resistance is a result of lower diffusion rates of fungal degradation agents through the wood cell wall. A recent paper explained the fundamental principles governing diffusion through the wood cell wall. This current paper summarizes the findings in that paper with respect to decay resistance of modified wood. In short, large scale motions of the amorphous polysaccharides of the wood cell wall are necessary for diffusion of degradation agents during incipient decay. Many wood modifications are likely preventing decay by preventing these motions. Water promotes large scale motions of cell wall polysaccharides by increasing free volume, increasing the distance between polymer chains, and reducing the number of hydrogen bonds between polymer chains.

Keywords: Decay resistance; diffusion; glass transition; molecular mobility; hemicellulose

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 302 kb(s)

Date posted: 06/30/2020

This publication is also viewable on Treesearch:  view
RITS Product ID: 98190
Current FPL Scientists associated with this product (listed alphabetically)
Hunt, Christopher G.
Research Chemist
Jakes, Joseph
Research Materials Engineer
Zelinka, Samuel L.
Materials Research Engineer

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »