Title: Utility of image software in quantification of termite damage on cross-laminated timber (CLT)

Source: In: Wang, X.; Sauter, U.H.; Ross, R.J., eds. 2019. Proceedings: 21st International Nondestructive Testing and Evaluation of Wood Symposium. General Technical Report FPL-GTR-272. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. pp 643-649.

Author(s)França, Tamara S.F.A.; Stokes, C. Elizabeth; Tang, Juliet D.; Arango, Rachel A.

Publication Year: 2019  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4723-2A

Abstract: Cross Laminated Timber (CLT) is part of a new generation of engineered wood products that are now widespread across Europe, Australia, and Canada. As this trend is now growing in the United States, manufacturers are looking to expand the use of CLT into the North American market, which includes states located in the southeastern U.S. As this region is known to have an increased risk of termite attack, standards should be developed to evaluate termite damage on CLT products prior to extensive use of the product in this region. However, existing standard test methods cannot be applied directly to CLT specimens as current standard test sample sizes are too small to adequately represent CLT constructed materials. Therefore, larger sample sizes were examined to determine resistance of CLT products against termite attack. Large sample size made it difficult to evaluate termite damage using weight loss as a variable as termite damaged specimens showed relatively low weight loss values. The objective of this work was to examine the use of the image analysis software, ImageJ, in determining the extent of termite damage on CLT blocks. Results showed that evaluation of void volume percent could be used in conjunction with weight loss and visual rating to obtain a more accurate measurement of overall termite damage in CLT.

Keywords: Mass timber products; subterranean termites; image measurements; mass loss

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 1,024 kb(s)

Date posted: 12/20/2019

This publication is also viewable on Treesearch:  view
RITS Product ID: 96765
Current FPL Scientist associated with this product
Tang, Juliet
Research Forest Products Technologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »