Title: Development of timber buckling restrained braces for mass timber braced frames

Source: In: Proceedings, 6th International network on timber engineering research conference, INTER/52-15-3. Tacoma, WA: 1-14.

Author(s)Murphy, Colton ; Pantelides, Chris ; Blomgren, Hans-Erik ; Rammer, Douglas

Publication Year: 2019  View PDF »

Category: Conference Proceedings

Abstract: Buckling Restrained Brace Frames (BRBF) are a proven and reliable method to provide an efficient lateral force resisting system for new and existing structures in earthquake prone regions. The fuse-type elements in this system facilitate stable energy dissipation at large load deformation levels. Currently, the new trend towards mass timber vertical structures creates a need for a lightweight compatible lateral force resisting system. A Buckling Restrained Brace (BRB) component is possible to construct and feasible to implement when combining a steel core with a mass timber casing herein named the Timber-Buckling Restrained Brace (T-BRB). T-BRBs when combined with mass timber beam and column elements can create a system that will have advantages over the current steel framed BRBF system when considering recyclability, sustainability, framing compatibility, and performance. This paper presents findings on small scale testing of candidate engineered wood products for the T-BRB casing and testing of six full scale 12 ft long 60 kip braces according to code prescribed loading protocols and acceptance criteria.

Keywords: Brace; buckling; building; damping; frame; fuse; seismic; structure; timber

Publication Review Process: Formally Refereed

File size: 3,072 kb(s)

Date posted: 11/01/2019

This publication is also viewable on Treesearch:  view
RITS Product ID: 96580
Current FPL Scientist associated with this product
Rammer, Douglas R.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »