Title: Ongoing field evaluation of Douglas-fir cross-laminated timber in a ground proximity protected test in Mississippi

Source: In: Proceedings, one hundred fourteenth annual meeting of the American wood protection association. Birmingham, AL: American Wood Protection Association: 132-137.

Author(s)Mankowski, Mark E., E. .; Shelton, Thomas G.; Kirker, Grant ; Morrell, Jeffrey J.

Publication Year: 2018  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4723-2A

Abstract: Current design standards incorporate the use of preservative treated and naturally durable wood where conditions are suitable for deterioration, but treatment options for mass timber products, particularly, cross laminated timber (CLT) remain to be addressed. Termiticide treatment is a necessity for CLT structures, especially in southeastern climates. Wood species currently used to fabricate CLT are non-durable, and current design standards do not properly address incorporation of preservative treatments into these systems. In this study, 12” x 14” x 4” Douglas-fir CLT pieces were installed in a ground proximity protected test at the Harrison Experimental Forest (HEF), (Saucier, MS). Test samples were placed in sets of two in 30” x 30” subplots on bricks approximately 3-4” above soil and covered with ventilated waterproof covers. A total of 20 test pairs (40 total samples) with four different treatments were installed. The treatments consisted of a soil termiticide treatment, a preventive borate spray treatment at initiation, a remedial treatment with the spray-on borate one year post initiation and untreated controls. Soil below five pairs of samples was treated the with a soil termiticide (Termidor® SC). For the preventive borate at initiation treatment, one sample per pair of five other sets was treated with a spray-on borate preventative treatment (Bora-Care®). The remaining ten pairs were left as untreated controls. Temperature and humidity inside some of the covered units is being monitored throughout the test. The ten control sets will be examined for termite attack 12 months after installation. Five of the attacked sets will be treated with spray-on borate as a remedial treatment for active termite attack.

Keywords: Cross-laminated timber; E21; ground proximity; soil termiticide; borate; field test; durability

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 3,072 kb(s)

Date posted: 04/04/2019

This publication is also viewable on Treesearch:  view
RITS Product ID: 93863
Current FPL Scientists associated with this product (listed alphabetically)
Kirker, Grant
Research Forest Products Technologist
Mankowski, Mark
Research Entomologist
Shelton, Thomas Guy
Research Entomologist

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »