Title: Multi-omic analyses of extensively decayed Pinus contorta reveal expression of a diverse array of lignocellulose-degrading enzymes

Source: Applied and Environmental Microbiology. 84(20): 1-41.

Author(s)Hori, Chiaki ; Gaskell, Jill ; Cullen, Dan ; Sabat, Grzegorz ; Stewart, Philip E.; Lail, Kathleen ; Peng, Yi ; Barry, Kerrie ; Grigoriev, Igor V; Kohler, Annegret ; Fauchery, Laure ; Martin, Francis ; Zeiner, Carolyn A.; Bhatnagar, Jennifer M.

Publication Year: 2018  View PDF »

Category: Journal Articles

Abstract: Fungi play a key role cycling nutrients in forest ecosystems but the mechanisms remain uncertain. To clarify the enzymatic processes involved in wood decomposition, metatranscriptomics and metaproteomics of extensively decayed lodgepole pine by RNAseq and LC-MS/MS, respectively. Following de novo metatranscriptome assembly, 52,011 were searched for functional domains and homology to database entries.

Keywords: Pinus contorta; wood decay; white rot; brown rot

Publication Review Process: Formally Refereed

File size: 1,024 kb(s)

Date posted: 10/02/2018

This publication is also viewable on Treesearch:  view
RITS Product ID: 92870
Current FPL Scientist associated with this product
Cullen, Daniel
Research Microbiologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »