Title: Full-scale fire tests of a two-story cross-laminated timber structure

Source: In: Proceedings, WCTE 2018-world conference on timber engineering. Seoul, Republic of South Korea: Korean Institute of Forest Science. 8 p.

Author(s)Hasburgh, Laura E.; Zelinka, Samuel L.; Bourne, Keith J.; Tucholski, David R.; Ouellette, Jason P.

Publication Year: 2018  View PDF »

Category: Conference Proceedings

Abstract: There is a current trend towards mid- and high-rise mass timber buildings. With this trend, there is a research need to develop a comparison between mass timber compartment fires and non-combustible compartment fires. In an effort to address the knowledge gaps in the fire performance of cross-laminated timber compartments, a full-scale fire test series was developed. The fire test series included five tests with varying levels of exposed cross-laminated timber on a two story cross-laminated timber structure. Here we present a detailed summary of the fire test series, instrumentation plan, and an overview of the results.

Keywords: Cross-laminated timber; full-scale fire test; timber construction; fire performance; compartment fire

Publication Review Process: Non-Refereed (Other)

File size: 1,024 kb(s)

Date posted: 09/27/2018
RITS Product ID: 92571
Current FPL Scientist associated with this product
Zelinka, Samuel L.
Materials Research Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »