Title: Internal moisture content and temperature of standardized aboveground wood durability test specimens

Source: Res. Paper FPL-RP-694. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 16 p.

Author(s)Lebow, Stan T.; Lebow, Patricia K.

Publication Year: 2018  View PDF »

Category: Research Papers
Associated Research Project(s):   FPL-4723-3A  FPL-4851-1B

Abstract: Durability of wood products intended for use in outdoor aboveground applications are evaluated using one or more standardized test methods. These methods use relatively small specimens in an effort to accelerate decay growth and allow detection of decay. In this study, we evaluated internal moisture content and temperature of standardized specimens and compared them with specimens of a simulated post and beam connection that is recommended for residential deck construction. Specimens of each type were cut from end-matched Southern Pine timbers and exposed above ground at a test site near Madison, Wisconsin. Pairs of stainless steel screws were inserted at multiple locations within each specimen to allow moisture content determination with a resistance-type moisture meter. Internal temperature was monitored in one specimen of each type using a thermistor probe and data logger. The specimens of the simulated post and beam connection sustained higher moisture contents and experienced less moisture content fluctuation than any of the standardized test specimens. Internal temperature also varied by specimen type but not to the extent observed for moisture content. The findings of this study suggest that frequent drying of standardized specimens has the potential to inhibit decay and may underestimate the decay hazard present within larger members of aboveground structures. Of the current standardized methods, the E18 ground proximity test appears to offer the best combination of relatively high moisture contents and ease of inspection. Other approaches, such as those that stack or layer groups of smaller specimens to entrap moisture and enhance decay, may warrant further consideration.

Keywords: Durability testing; aboveground; standardized specimens; moisture content; temperature

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 931 kb(s)

Date posted: 08/14/2018

This publication is also viewable on Treesearch:  view
RITS Product ID: 91111
Current FPL Scientists associated with this product (listed alphabetically)
Lebow, Patricia K.
Mathematical Statistician
Lebow, Stan T.
Research Forest Products Technologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »