Title: Post-sulfonation of cellulose nanofibrils with a one-step reaction to improve dispersibility

Source: Carbohydrate Polymers. 181: 247-255.

Author(s)Luo, Jeffrey; Semenikhin, Nikolay; Chang, Huibin; Moon, Robert J.; Kumar, Satish

Publication Year: 2018  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4707-3B

Abstract: Cellulose nanofibrils (CNF) were sulfonated and the dispersion quality was compared to unfunctionalized and 2,2,6,6-tetramethylpiperdine-1-oxyl radical (TEMPO) post-oxidation treatment of existing CNF (mechanically fibrillated pulp). A post-sulfonation treatment on existing CNF in chlorosulfonic acid and dimethylformamide (DMF) resulted in sulfonated CNF that retained a fibril-like morphology. There was a small decrease in the cellulose crystallinity index for the sulfonated CNF, but this was much lower than the reported regioselective oxidative bisulfite pretreatment method used to make sulfonated CNF. The current approach was extremely quick, and 5 min of reaction time was sufficient to result in significant improvements in dispersibility compared to unfunctionalized CNF. The sulfonated CNF and TEMPO oxidized CNF had better dispersibility compared to the unfunctionalized CNF when dispersed in DMF and water, and in many cases the sulfonated CNF had better dispersibility than the TEMPO CNF. It was found that when CNF was dispersed in DMF the TEMPO CNF formed carboxyl dimethylammonium groups, while the sulfonated CNF formed formate groups.

Keywords: Cellulose sulfate; cellulose nanofibrils; cellulose

Publication Review Process: Formally Refereed

File size: 1,024 kb(s)

Date posted: 03/29/2018

This publication is also viewable on Treesearch:  view
RITS Product ID: 89855
Current FPL Scientist associated with this product
Moon, Robert J.
Materials Research Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »