Title: Residential tornado safe room from commodity wood products – design and development

Source: Gen. Tech. Rep. FPL-GTR-253. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 1-8.

Author(s)Falk, Robert H.; Bridwell, James J.

Publication Year: 2018  View PDF »

Category: General Technical Reports
Associated Research Project(s):   FPL-4714-3B

Abstract: In the United States, tornadoes cause significant damage and result in many injuries and deaths. Although the development and use of tornado safe rooms have helped decrease the human toll associated with these events, the cost of these structures is often too high for many that could benefit from their use. The development of a nonproprietary residential tornado safe room constructed from commodity wood building products, buildable by a local contractor or do-it-yourselfer, and adaptable to existing homes, could lower the cost of these structures and result in more widespread use. This report is an overview of the design and development of such a residential tornado safe room. This design was tested according to the requirements of the International Code Council Standard for the Design and Construction of Storm Shelters. It has a projected material cost of between $3,500 and $4,000, which is significantly less than a prefabricated room of similar size and built from other materials.

Keywords: Tornado safe room; design; wood construction

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 1,024 kb(s)

Date posted: 03/19/2018

This publication is also viewable on Treesearch:  view
RITS Product ID: 89751
Current FPL Scientist associated with this product
Falk, Robert H.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »