Title: Long term durability of wood-plastic composites made with chemically modified wood

Source: In: Advancements in fiber-polymer composites conference proceedings. Madison, WI: 1-17.

Author(s)Ibach, Rebecca E.; Clemons, Craig M.

Publication Year: 2017  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4706-2B   FPL-4707-1B

Abstract: Wood-plastic composites (WPCs) have slower moisture sorption than solid wood, but over time moisture can impact the strength, stiffness, and decay of the composite. These changes will become increasingly important if WPCs are used in more challenging environments such as in ground-contact applications. There are several options for mitigating the moisture sorption of WPCs. A coupling agent can be added to potentially improve the wetting and dispersion of the wood flour and improve its adhesion with the plastic matrix. In previous investigations, the use of a coupling agent has been shown to further slow, though not stop, moisture intrusion in WPCs. Alternatively, the wood flour can be chemically modified to make the wood itself more hydrophobic and, therefore, reduce the driving force for moisture intrusion rather than just slow it.

While the effects of such approaches to moisture reduction have been investigated somewhat in the laboratory setting, field exposure is ultimately needed to verify the overall long-term durability of such WPCs, which includes the potentially synergistic effects of exposure to sunlight, moisture, wind, temperature fluctuations, freeze/thaw, wet/dry cycling, termites, mold and decay fungi. WPCs containing either a coupling agent or chemically modified wood flour were fabricated. These modified WPCs and a control were installed both above-ground and in-ground in Saucier, Mississippi and Madison, Wisconsin and observations (e.g., appearance, thickness swell, and fungal attack) were recorded over a 12 year time period. Results will be discussed, as well as correlation between laboratory and field measurements.

Keywords: Acetylation; coupling agent; moisture sorption; fungal decay; extrusion; field exposure

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 432 kb(s)

Date posted: 09/27/2017

This publication is also viewable on Treesearch:  view
RITS Product ID: 87009
Current FPL Scientists associated with this product (listed alphabetically)
Clemons, Craig M.
Materials Research Engineer
Ibach, Rebecca E.
Research Chemist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »