Title: Energy harvesting from wood floor vibration using a piezoelectric generator

Source: Research Note, FPL–RN–0347. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 9 p.

Author(s)Kan, Jiangming; Ross, Robert J.; Wang, Xiping; Li, Wenbin

Publication Year: 2017  View PDF »

Category: Research Notes
Associated Research Project(s):   FPL-4714-1B

Abstract: Vibration can occur in wood floor systems as a consequence of a variety of human activities, ranging from common daily movements associated with individuals living in homes to high-intensity activities associated with sporting events that are held in large sports arenas. For example, the potential for harvesting energy from a wooden floor system in public buildings during daily rush hours could be substantial. In this pilot study, an energy harvesting system was developed to investigate the feasibility of harvesting energy from a vibrating wooden floor system. The purpose of this publication is to provide a summary of the experimental technique we developed and to present data obtained from its use.

Keywords: Energy harvesting; piezoelectric property; vibration; wood floor systems

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 1,024 kb(s)

Date posted: 06/30/2017

This publication is also viewable on Treesearch:  view
RITS Product ID: 85004
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Wang, Xiping
Research Forest Products Technologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »