Title: Lateral testing of glued laminated timber tudor arch

Source: World Conference on Timber Engineering, WCTE 2016, August 22-25.

Author(s)Rammer, Douglas R.; Line, Philip

Publication Year: 2016  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4714-3B

Abstract: Glued laminated timber Tudor arches have been in wide use in the United States since the 1930s, but detailed knowledge related to seismic design in modern U.S. building codes is lacking. FEMA P-695 (P-695) is a methodology to determine seismic performance factors for a seismic force resisting system. A limited P-695 study for glued laminated timber arch structures highlighted the lack of lateral load testing; therefore, critical modelling information was not available and assumptions based on available research were used. In this study, full-scale lateral load testing of the glued laminated timber arch is used to fill in gaps in test-based information and assess the following characteristics: damping, deformation behaviour, and failure modes.

Keywords: Glued Laminated Timber, Arches, Seismic Design, Experiential, Failure

Publication Review Process: Formally Refereed

File size: 1,024 kb(s)

Date posted: 03/01/2017

This publication is also viewable on Treesearch:  view
RITS Product ID: 84180
Current FPL Scientist associated with this product
Rammer, Douglas R.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »