Title: Nanocellulose in spun continuous fibers: A review and future outlook

Source: Journal of Renewable Materials, Vol. 4(5): 327-339

Author(s)Clemons, Craig

Publication Year: 2016  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-1B

Abstract: Continuous fibers are commonly manufactured for a wide variety of uses such as filters, textiles, and composites. For example, most fibrous reinforcements (e.g., carbon fiber, glass fiber) for advanced composites are continuous fibers or yarns, fabrics, and preforms made from them. This allows broad flexibility in design and manufacturing approaches by controlling fiber orientation and architecture. However, there has been growing interest in preparing continuous fibers from biobased materials such as plants. Of particular recent interest are nanocelluloses, which are projected to be less expensive than many other nanomaterials and have the potential to be produced in large volumes. They also have an impressive strength-to-weight ratio and have so far shown few environmental, health, and safety concerns in their unmodified state. However, efficient and effective use of nanocellulose in continuous fibers is challenging and a variety of approaches have been explored in which nanocellulose dispersions are either spun directly or in combination with polymers. Methods such as wet spinning, dry spinning melt spinning, and electrospinning have been investigated. To better understand the body of knowledge of this new and growing area, various approaches are reviewed and a perspective on what the future holds is provided.

Keywords: Nanocellulose, cellulose nanofibrils, cellulose nanocrystals, fiber, spinning

Publication Review Process: Formally Refereed

Date posted: 12/20/2016

This publication is also viewable on Treesearch:  view
RITS Product ID: 83777
Current FPL Scientist associated with this product
Clemons, Craig M.
Materials Research Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »