Title: Live-load performance evaluation of historic covered timber bridges in the United States

Source: Journal of Performance of Constructed Facilities, 2016, 30(4).

Author(s)Seo, Junwon; Hosteng, Travis K.; Phares, Brent M.; Wacker, James P.

Publication Year: 2015  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4714-3B

Abstract: The National Historic Covered Bridge Preservation Program (NHCBP), sponsored by the Federal Highway Administration (FHWA), was established to preserve the covered timber bridge structures that were constructed in the early 1800s. Today, many of the approximately 880 covered timber bridges still in existence in the United States are closed to vehicular traffic; furthermore, a large percentage of the remaining bridges open to traffic are restricted by load postings. Unfortunately, there are no current load-rating standards for covered timber bridges, so engineers do not have many resources at their disposal to reliably understand the behavior of these complex structures. As a result, the estimated load postings and/or ratings are often too conservative. To better understand the live-load performance of covered timber bridges and to develop improved criteria for their load ratings, a series of live-load tests were performed on 11 single-span, historic covered timber bridges. This paper explains the field testing conducted on all of the bridges, and makes recommendations for the conduct of other similar tests. The tests consisted of installing a network of multiple displacement and strain sensors on the structures, and monitoring global displacements and member strains at various cross sections during passage of a known test. The vehicle used in the testing met the load restrictions in place at the time of testing. The results of this work serve as a basis for instrumentation and field testing, to investigate the liveload performance on such bridges. This paper outlines the field-testing methods and summarizes the results from the testing of all 11 bridges. Based on the field-testing methods, a field-testing protocol is recommended for the live-load testing of historic covered timber bridges. Feasibility of the recommended protocol is also evaluated using a finite-element model analysis for a selected bridge among the tested bridges.

Keywords: Field testing,Live-load performance,Timber,Covered bridges,Burr arch truss,Howe truss,Queen post truss

Publication Review Process: Formally Refereed

File size: 9,216 kb(s)

Date posted: 09/26/2016

This publication is also viewable on Treesearch:  view
RITS Product ID: 81997
Current FPL Scientist associated with this product
Wacker, James P.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »