Title: Laboratory Evaluations of Durability of Southern Pine Pressure Treated With Extractives From Durable Wood Species

Source: Journal of Economic Entomology

Author(s)Kirker, Grant T.; Blodgett, Amy; Lebow, Patricia

Publication Year: 2015  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4723-1A  FPL-4851-1B

Abstract: Extracts from sawdust of four naturally durable wood species [Alaskan yellow cedar, AYC, Cupressus nootkanansis D. Don 1824; eastern red cedar, ERC, Juniperus virginiana L.; honey mesquite, HM, Prosopis glandulosa Torr.; and black locust, BL, Robinia pseudoacacia L.] were used to treat southern pine, Pt, Pinus taeda L. sapwood blocks. Extractive treated blocks were evaluated for decay resistance in standard soil bottle fungal assays challenged with brown and white rot decay fungi. Results showed that extractives did impart some improvement to decay resistance of Pt blocks. BL- and HM-treated Pt blocks were also used in choice and no-choice assays to determine feeding preference and damage by eastern subterranean termites (Reticulitermes flavipes) Kollar. Minimal feeding on treated blocks was seen in both choice and no-choice assays. In choice assays, there was similar mortality between HM and BL arenas; however, in no-choice assays, complete mortality was recorded for HM-treated Pt and high mortality was seen with BL-treated Pt. Subsequent dose mortality termite assays showed HM to be effective in killing R. flavipes at low concentrations. Both HM and BL show promise as deterrents or termiticidal protectants and will be further evaluated in field studies.

Keywords: wood; durability; Reticulitermes flavipes; feeding; extractives

Publication Review Process: Formally Refereed

File size: 647 kb(s)

Date posted: 07/12/2016

This publication is also viewable on Treesearch:  view
RITS Product ID: 79530
Current FPL Scientists associated with this product (listed alphabetically)
Kirker, Grant
Research Forest Products Technologist
Lebow, Patricia K.
Mathematical Statistician
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »