Title: Ultrasound Transmission Times in Biologically Deteriorated Wood

Source: In: Proceedings: 19th International Nondestructive Testing and Evaluation of Wood Symposium. 14 p.

Author(s)Senalik, Christopher Adam; Ross, Robert J.; DeGroot, Rodney

Publication Year: 2015  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4714-1B

Abstract: The use of a variety of stress wave transmission techniques for the in-service condition assessment of deteriorated wood is well documented. This paper summarizes results from an extensive study designed to examine the relationship between ultrasound transmission times and the deterioration of exposed wood. Two hundred seventy (270) southern pine lumber specimens were evaluated nondestructively using a through transmission ultrasound technique after field exposure for periods of up to fifty seven (57) months. Ultrasound transmission times increased with exposure time. Several statistical models of the relationship between transmission time and length of exposure were developed and are presented.

Keywords: International Nondestructive Testing and Evaluation of Wood Symposium; nondestructive testing; nondestructive evaluation; wood; wood products

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 368 kb(s)

Date posted: 05/19/2016

This publication is also viewable on Treesearch:  view
RITS Product ID: 79227
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Senalik, Christopher
Research General Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »