Title: Changes in bark composition from long-term elevated CO2 treatment: Implications for the management of sweetgum as a wood energy crop

Source: In: Proceedings of the 18th biennial southern silvicultural research conference. e–Gen. Tech. Rep. SRS–212. Asheville, NC: U.S. Department of Agriculture, Forest Service, Southern Research Station

Author(s)Eberhardt, Thomas L.; So, Chi-Leung; Labbé, Nicole; Leduc, Daniel J.; Warren, Jeffrey M.

Publication Year: 2016  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4715-1

Abstract: Tree bark is comprised of living inner bark (phloem) that transports the products of photosynthesis and dead outer bark that protects the living tissues and seals in moisture. Active and passive defenses against destructive agents (e.g., insects, fungal pathogens) are provided by the inner bark and outer bark, respectively (Eberhardt 2013). For sweetgum (Liquidambar styraciflua L.), the bark comprises 23 percent by mass of the sapling-sized stems and 31 percent of the branches (Koch 1985); the percentage of bark in larger trees would be less. Trees debarked during processing by the forest products industry sector generate significant amounts of bark residue for conversion to mulch products or for fuel value recovery. The chemical composition of tree bark is important as it has the potential to significantly impact the utilization of bark, particularly for biofuel applications.

Keywords: climate change, phloem, rhytidome, biomass

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 504 kb(s)

Date posted: 04/29/2016

This publication is also viewable on Treesearch:  view
RITS Product ID: 79066

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »