Title: Microwave flexible transistors on cellulose nanofibrillated fiber substrates

Source: Applied Physics Letters

Author(s)Seo, Jung-Hun; Chang, Tzu-Hsuan; Lee, Jaeseong; Sabo, Ronald; Zhou, Weidong; Cai, Zhiyong; Gong, Shaoqin; Ma, Zhenqiang

Publication Year: 2015  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-2B

Abstract: In this paper, we demonstrate microwave flexible thin-film transistors (TFTs) on biodegradable substrates towards potential green portable devices. The combination of cellulose nanofibrillated fiber (CNF) substrate, which is a biobased and biodegradable platform, with transferrable single crystalline Si nanomembrane (Si NM), enables the realization of truly biodegradable, flexible, and high performance devices. Double-gate flexible Si NM TFTs built on a CNF substrate have shown an electron mobility of 160 cm2/V•s and ƒT and ƒmax of 4.9GHz and 10.6 GHz, respectively. This demonstration proves the microwave frequency capability and, considering today’s wide spread use of wireless devices, thus indicates the much wider utility of CNF substrates than that has been demonstrated before. The demonstration may also pave the way toward portable green devices that would generate less persistent waste and save more valuable resources

Keywords: Cellulose Nanofibrils; Thin film transistors (TFTs); flexible electronics; silicon nanomembrane (Si NM); biodegradable

Publication Review Process: Formally Refereed

File size: 2,048 kb(s)

Date posted: 01/07/2016

This publication is also viewable on Treesearch:  view
RITS Product ID: 78069
Current FPL Scientists associated with this product (listed alphabetically)
Cai, Zhiyong
Supervisory Research Materials Engineer
Sabo, Ronald C.
Research Materials Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »