Title: Kiln drying of White fir

Source: Reprinted from the August, 1947, issue of West Coast Lumberman Volume 74, 1947; 2 p.

Author(s): Smith, H.H.

Publication Year: 1947  View PDF »

Category: Journal Articles

Abstract: The kiln drying of white fir (Abies concolor) was studied as a part of a broad utilization program for this species undertaken by the Forest Products Laboratory in cooperation with the California Forest and Range Experimental Station. The relatively low price of white fir lumber has encouraged the use of severe commercial drying schedules in order to reduce its drying time to a minimum, and drying defects have been reported from use of such schedules. The purpose of this study was to develop a kiln schedule bywhich white fir could be dried rapidly to a final moisture content of 12 to 14 percent without objectionable defects.

Keywords: abies concolor, kiln drying

Publication Review Process: Non-Refereed (Other)

File size: 776 kb(s)

Date posted: 10/28/2015
RITS Product ID: 77692

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »