Title: Using a combined hydrolysis factor to optimize high titer ethanol production from sulfite-pretreated poplar without detoxification

Source: Bioresource Technology. 186: 223-231.

Author(s)Zhang, Jingzhi; Gu, Feng; Zhu, J.Y.; Zalesny Jr., Ronald S., Jr..

Publication Year: 2015  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4709-1B

Abstract: Sulfite pretreatment to overcome the recalcitrance of lignocelluloses (SPORL) was applied to poplar NE222 chips in a range of chemical loadings, temperatures, and times. The combined hydrolysis factor (CHF) as a pretreatment severity accurately predicted xylan dissolution by SPORL. Good correlations between CHF and pretreated solids enzymatic digestibility, sugar yield, and the formations of furfural and acetic acid were obtained. Therefore, CHF was used to balance sugar yield with the formation of fermentation inhibitors for high titer ethanol production without detoxification. The results indicated that optimal sugar yield can be achieved at CHF = 3.1, however, fermentation using un-detoxified whole slurries of NE222 pretreated at different severities by SPORL indicated CHF ≈  2 produced best results. An ethanol titer of 41 g/L was achieved at total solids of approximately 20 wt% without detoxification with a low cellulase loading of 15 FPU/g glucan (27 mL/kg untreated wood).

Keywords: Poplar woods; Cellulosic biofuel; High solids processing; Fermentation inhibition; Pretreatment optimization

Publication Review Process: Formally Refereed

File size: 480 kb(s)

Date posted: 04/08/2015

This publication is also viewable on Treesearch:  view
RITS Product ID: 72584
Current FPL Scientist associated with this product
Zhu, JunYong
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »