Title: Effective of Microwave-KOH Pretreatment on Enzymatic Hydrolysis of Bamboo

Source: Journal of Sustainable Bioenergy Systems, Volume 2, 2012; pp. 104-107.

Author(s)Li, Zhiqiang; Jiang, Zehui; Yu, Yan; Cai, Zhiyong

Publication Year: 2012  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-1B

Abstract: Bamboo, with its advantages of fast growth, short renovation, easy propagation and rich in cellulose and hemicellulose, is a potential feedstock for bioethanol or other biofuels production. The objective of this study was to examine the fea- sibility of microwave assistant KOH pretreatments to enhance enzymatic hydrolysis of bamboo. Pretreatment was car- ried out by immersing the bamboo in KOH (12% and 8% w/w bamboo) solutions and exposing the slurry to microwave radiation power of 400 W for 30min. Chemical composition of the pretreated substrates and spent liquor was analyzed. Pretreated substrates were enzymatic hydrolyzed, and glucose and xylose in the hydrolysate were analyzed. The results showed that the pretreated substrate with microwave assisted KOH had significantly higher sugar yield than the un- treated samples. The fermentation inhibitors formic acid, furfural, HMF and levulinic acid were much lower than acid pretreatment reported

Keywords: Bamboo; Microwave-KOH Pretreatment; Chemical Pretreatment; Enzymatic Hydrolysis; Bioethanol Production

Publication Review Process: Formally Refereed

File size: 104 kb(s)

Date posted: 01/20/2015

This publication is also viewable on Treesearch:  view
RITS Product ID: 71851
Current FPL Scientist associated with this product
Cai, Zhiyong
Supervisory Research Materials Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »