Title: Nondestructive Testing Technique to Quantify Deterioration from Marine Borer Attack in Sitka Spruce and Western Hemlock Logs: Observations from a Pilot Test

Source: USDA Forest Service, Forest Products Laboratory, Research Note, FPL-RN-0333, 2014; 8 p.

Author(s)Ross, Robert; Forsman, John W.; Erickson, John R.; Brackley, Allen M.

Publication Year: 2014  View PDF »

Category: Research Notes
Associated Research Project(s):   FPL-4714-1B

Abstract: Stress-wave nondestructive evaluation (NDE) techniques are used widely in the forest products industry—from the grading of wood veneer to inspection of timber structures. Inspection professionals frequently use stress-wave NDE techniques to locate internal voids and decayed or deteriorated areas in large timbers. Although these techniques have proven useful, little information exists concerning the relationship between stress-wave parameters and deterioration observed as a consequence of marine borer attack. In this pilot test, we examined the relationship between stress-wave transmission time and the quality of wood in Sitka spruce and western hemlock logs that had varying degrees of deterioration as a consequence of attack from marine borers. Stress-wave transmission time, perpendicular to grain, was measured at several locations on each log. The logs were then sawn into lumber, which was then visually evaluated. A relationship was observed between stress-wave transmission time and deterioration of the logs and the yield of lumber from the logs.

Keywords: Nondestructive testing; Sitka spruce; western hemlock; marine borer; stress waves

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 335 kb(s)

Date posted: 12/23/2014

This publication is also viewable on Treesearch:  view
RITS Product ID: 71741
Current FPL Scientist associated with this product
Ross, Robert J.
Supervisory Research Gen. Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »