Title: High Strength Wood-based Sandwich Panels reinforced with fiberglass and foam

Source: BioResources, Volume 9, Number 2, 2014; pp. 1898-1913.

Author(s)Li, Jinghao; Hunt, John F.; Gong, Shaoqin; Cai, Zhiyong

Publication Year: 2014  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-2B

Abstract: Mechanical analysis is presented for new high-strengthsandwich panels made from wood-based phenolic impregnated laminated paper assembled with an interlocking tri-axial ribbed core. Four different panel configurations were tested, including panels with fiberglass fabric bonded to both outside faces with self-expanding urethane foam used to fill the ribbed core. The mechanical behaviors of the sandwich panels were strength tested via flatwise compression, edgewise compression, and third-point load bending. Panels with fiberglass exhibited significantly increased strength and apparent MOE in edgewise compression and bending, but there were no noticeable effects in flatwise compression. The foam provided improved support that resisted both rib buckling and face buckling for both compression and bending tests. Post-failure observation indicated that core buckling dominated the failures for all configurations used. It is believed that using stiffer foam or optimizing the dimension of the core might further improve the mechanical performance of wood-based sandwich panels.

Keywords: Wood-based Laminate paper; Foams; Glass fibers; Sandwich structure; Mechanical testing

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 542 kb(s)

Date posted: 12/22/2014

This publication is also viewable on Treesearch:  view
RITS Product ID: 71731
Current FPL Scientists associated with this product (listed alphabetically)
Cai, Zhiyong
Supervisory Research Materials Engineer
Hunt, John F.
Research General Engineer

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »

Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »

Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »

Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »