Title: Chapter 66: Strength properties of composites from biobased and synthetic fibers

Source: In: Cellulosics: Chemical, Biochemical and material aspects. New York: Ellis Horwood. 1993. Chapter 66; 1993; pp. 453-458.

Author(s)Young, R.A.; Rowell, R.M.; Sanadi, A.; Clemons, C.

Publication Year: 1993  View PDF »

Category: Book Chapter

Abstract: Biobased composites have been produced from esterified aspen fibers with either a thermosetting (phenol-formaldehyde, PF) or thermoplastic (polypropylene) matrix material. The polypropylene was incorporated in fibrous form. The level of esterification of the wood fibers had the greatest effect on the strength properties of PF bonded fiberboards, while the type of esterifying agent, acetic anhydride, maleic anhydride or succinic anhydride, had little or no effect. Acetylation of aspen fibers did not appear to increase the compatibility of the aspen fibers with polypropylene.

Keywords: composite boards, fiberboards, mechanical properties, strength

Publication Review Process: Non-Refereed (Other)

File size: 187 kb(s)

Date posted: 11/18/2014
RITS Product ID: 71596
Current FPL Scientist associated with this product
Clemons, Craig M.
Materials Research Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »