Title: Lignin-based Phenol-Formaldehyde Resins from Purified CO2 Precipitated Kraft lignin (PCO2KL)

Source: In: International Conference on Wood Adhesives, October 9-11, 2013 Toronto, Ontario Canada from CD ISBN: 978-0-935018-37-0; 2013; pp. 601-610.

Author(s)Chen, Yao; Frihart, Charles R.; Cai, Zhiyong; Lorenz, Linda F.; Stark, Nicole M.

Publication Year: 2013  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4706-1B  FPL-4707-2B

Abstract: To investigate the potential for using purified CO2-precipitated Kraft lignin (PCO2KL) with phenol-formaldehyde (PF) for application as an adhesive in plywood production, two lignin replacement procedures were examined to assess lignin’s effect on bond quality. Methylolation and oxidation with hydrogen peroxide (H2O2) were carried out to try to increase lignin reactivity. The first procedure involved substitution of 30% of the PF resin solids in the adhesive mix with a solution of methylolated lignin with or without prior oxidation; the second replacement procedure involved direct condensation of lignin or oxidized lignin to replace 25% of phenol. Formulated adhesives were compared to a control phenol-formaldehyde (PF) adhesive prepared in the laboratory. The physical properties (solid content, viscosity and pH values) of formulated resins were determined. PCO2KL-based adhesives showed comparatively good plywood shear strengths. However, they had lower wood failures than those of test samples made from PF resin only.

Keywords: Kraft lignin, lignin-phenol-formaldehyde resin, hydrogen peroxide, methylolation, physical properties, shear strength, wood failure

Publication Review Process: Informally Refereed (Peer-Reviewed)

Date posted: 10/17/2014

This publication is also viewable on Treesearch:  view
RITS Product ID: 69697
Current FPL Scientists associated with this product (listed alphabetically)
Cai, Zhiyong
Supervisory Research Materials Engineer
Frihart, Charles R.
Research Chemist
Stark, Nicole M.
Research Chemical Engineer

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »