Title: Fe-catalyzed thermal conversion of sodium lignosulfonate to graphene

Source: Materials Letters, 100, 2013; pp. 180-183.

Author(s)Mun, Sung Phil; Cai, Zhiyong; Zhang, Jilei

Publication Year: 2013  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-2B

Abstract: Sodium lignosulfonate (LS) from sulfite pulping processing was used as a carbon source to synthesize graphene. LS was mixed with Fe nanoparticles (FeNPs) as a catalyst and thermally treated at 1000 °C for 1 h. The Raman spectrum and X-ray diffraction pattern suggested that graphene sheets were formed in LS thermally treated with FeNPs (Fe-HTLS). Scanning electron microscopy image of Fe-HTLS showed clusters of thin graphene sheets appearing in the form of nanoflowers. High-resolution transmission electron microscopy and electron reflection images provided further evidence of the formation of graphene in LS thermally treated in the presence of Fe catalyst.

Keywords: Lignosulfonate; Sulfite pulping; Fe nanoparticles; Graphene; Thermal treatment; Raman spectrum

Publication Review Process: Formally Refereed

File size: 597 kb(s)

Date posted: 09/25/2014

This publication is also viewable on Treesearch:  view
RITS Product ID: 69483
Current FPL Scientist associated with this product
Cai, Zhiyong
Supervisory Research Materials Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »