Title: Localized Notch Reinforcement for Wooden Beams

Source: U.S. Patent 5,852,909. Dec 29, 1998. 5 p. Int. Classif. E04C 5/07.https://patents.google.com/patent/US5852909A/en?oq=08%2f943%2c367

Author(s)Soltis, Lawrence A.; Ross, Robert J.; Rammer, Douglas R.

Publication Year: 2014  View Document »

Category: Patents

Abstract: A localized fiber reinforcement places strong tensile strength fibers across a hypothetical split line near notches in beams to curtail split propagation caused by cross-grain tension that may otherwise significantly reduce the strength of a beam used as a spanning member. An adhesive coated patch may be applied after a notch is cut in the beam or fibers may be attached to a beam at a factory near the location of an anticipated notching.

Keywords: fiber reinforcement, tensile strength fibers, wooden structure members, beam, adhesive, fiber patch

Date posted: 09/22/2014
RITS Product ID: 69230
Current FPL Scientists associated with this product (listed alphabetically)
Rammer, Douglas R.
Research General Engineer
Ross, Robert J.
Supervisory Research Gen. Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »