Title: Color and Surface Chemistry Changes of Pine Wood Flour after Extraction and Delignification

Source: BioResources, Volume 9, Number 2, 2014; pp. 2937-2948.

Author(s)Chen, Yao; Tshabalala, Mandla A.; Gao, Jianmin; Stark, Nicole M.; Fan, Yongming

Publication Year: 2014  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-1B  FPL-4707-2B

Abstract: A detailed study was undertaken to examine the color and chemistry changes of pine wood flour when its extractives are removed and when it is delignified. The solvent systems employed were toluene/ethanol (TE), acetone/water (AW), and hot-water (HW), while sodium chlorite/acetic acid were used for delignification (i.e., lignin removal (LR)). Samples were analyzed by attenuated total reflectance-Fourier transform infrared (ATR-FTIR) spectroscopy, Fourier transform Raman (FT-Raman) spectroscopy, and colorimetry. The study demonstrated that color parameters (i.e., CIE L a b ) were only slightly affected by the removal of extractives, but changed noticeably when extractions were followed by delignification. TE extraction was more effective at removing the yellow colored substances, whereas AW mostly removed red colored substances that contained C=O groups. Inclusion of a HW extraction step after extraction with AW (AW-HW) removed components that contained conjugated C=O structures. Inclusion of a delignification step after extraction with AW followed by HW extraction (AW-HW-LR) was effective at removing yellow substances that contained non-conjugated C=O groups

Keywords: Wood flour, Extractives, Lignin, Surface chemistry, Color, Extractives, Delignification

Publication Review Process: Formally Refereed

File size: 355 kb(s)

Date posted: 08/04/2014

This publication is also viewable on Treesearch:  view
RITS Product ID: 68128
Current FPL Scientists associated with this product (listed alphabetically)
Stark, Nicole M.
Research Chemical Engineer
Tshabalala, Mandla A.
Research Chemist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »