Title: The effects of copper proximity on oxalate production in Fibroporia radiculosa

Source: The International Research Group on wood Protection, section 1, Biology, IRG/WP 14-10823; 2014; pp. 2-12.

Author(s)Jenkins, Katie M.; Clausen, Carol A.; Green III, Frederick

Publication Year: 2014  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4723-4B

Abstract: Copper remains a key component used in wood preservatives available today. However, the observed tolerance of several critical wood rotting organisms continues to be problematic. Tolerance to copper has been linked to the production and accumulation of oxalate, which precipitates copper into insoluble copper-oxalate crystals, thus inactivating copper ions. The purpose of this study was to assess differences in oxalate production and decay capacity of four wood decay fungi (three copper-tolerant and one copper-sensitive) exposed to various applications of copper. Three Fibroporia radiculosa isolates and one Gloeophyllum trabeum isolate were subjected to one formulation of copper citrate presented to the test fungi by four different treatments in Southern pine wood blocks for an eight week period. Samples were evaluated for oxalate production and weight loss every two weeks. Two of the copper-tolerant isolates evaded the inhibitory effects of all four copper treatments by week eight. The copper-sensitive organism exhibited some limitations to actively decay blocks in two of the four copper treatments. These findings suggest that proximity to copper citrate, available in any form (i.e. impregnation, direct contact, free liquid or close proximity) generally, had no negative effect on fungal growth, oxalate production, and decay capacity of the copper-tolerant organisms. Results also suggested that the copper-sensitive fungus was restricted in its ability to effectively decay wood when copper was pressure treated or directly added to the surface of wood blocks. This study also suggested that close proximity to copper alone (i.e. not pressure treated) did not completely inhibit decay of the copper-tolerant or copper-sensitive test fungi.

Keywords: brown-rot decay; copper-tolerance; oxalate; Fibroporia; proximity to copper

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 172 kb(s)

Date posted: 07/18/2014

This publication is also viewable on Treesearch:  view
RITS Product ID: 67962
Current FPL Scientists associated with this product (listed alphabetically)
Clausen, Carol A.
Supervisory Research Microbiologist
Green, Frederick
Research Microbiologist
Ohno, Katie
Research Biologist

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »