Title: Structural Evaluation of the Second Oldest Glued-Laminated Structure in the United States

Source: USDA Forest Service, Forest Products Laboratory, General Technical Report, FPL-GTR-226. pp. 269-276.

Author(s)Rammer, Douglas R.; Moura, Jorge de Melo

Publication Year: 2013  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4714-2B

Abstract: The second glued-laminated structure built in the United States was constructed at the USDA Forest Products Laboratory (FPL) in 1934 to demonstrate the performance of wooden arch buildings. After decades of use the structure was decommissioned in 2010. Shortly after construction, researchers structurally evaluated the glued-laminated arch structure for uniform loading on the center arch. This structural system evaluation was added to the existing laboratory work on glued-laminated arches to develop the foundation on which the current glued-laminated arch design criteria is based. After decommisioning, recovered arches were tested in the laboratory to evaluate the loss of structural performance. Loss of structural performance was evaluated by comparing original and current deformation. Based on a preliminary visual and structural assessment, the degradation of structural performance was minimal in the arches, except for one arch that was exposed to a significant amount of water resulting from fighting a building fire.

Keywords: glued-laminated; arch; historical; structural evaluation; ultrasound

Publication Review Process: Formally Refereed

File size: 763 kb(s)

Date posted: 10/24/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 66561
Current FPL Scientist associated with this product
Rammer, Douglas R.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »