Title: Analysis of Wave Velocity Patterns in Black Cherry Trees and its Effect on Internal Decay Detection

Source: In: Gen. Tech. Rept. FPL-GTR-226. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. p. 224-232.

Author(s)Li, Guanghui; Wang, Xiping; Wiedenbeck, Jan; Ross, Robert J.

Publication Year: 2013  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4714-1B

Abstract: In this study, we examined stress wave velocity patterns in the cross sections of black cherry trees, developed analytical models of stress wave velocity in sound healthy trees, and then tested the effectiveness of the models as a tool for tree decay diagnosis. Acoustic tomography data of the tree cross sections were collected from 12 black cherry trees at a production forest. Trees were subsequently cut, and the disk at each test location was obtained to assess the true physical condition. Stress wave velocity data of different paths across grain, from radial to tangential, were extracted from the acoustic tomography data sets. our analysis indicated that the ratio of tangential velocity to radial velocity in sound healthy trees approximated a second-order parabolic curve with respect to the symmetric axis θ = 0 (θ is the angle between wave propagation path and radial direction). The analytical model was found in excellent agreement with the real data from healthy trees. Further examination indicated that the analytical model can be used to diagnose internal conditions of trees when a stress wave testing method is used in tree inspection.

Keywords: stress wave, velocity pattern, trees, internal decay detection, tomography

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 1,653 kb(s)

Date posted: 10/24/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 66556
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Wang, Xiping
Research Forest Products Technologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »