Title: Chapter 2.3 Cellulose Nanofibril Composite Substrates for Flexible Electronics

Source: In: Production and applications of Cellulose Nanomaterials, Chapter 2.3, TAPPI Press 2013; pp. 263-264.

Author(s)Sabo, Ronald; Seo, Jung-Hun; Ma, Zhenqiang

Publication Year: 2013  View PDF »

Category: Book Chapter
Associated Research Project(s):   FPL-4706-2B

Abstract: Flexible electronics have a large number of potential applications, including malleable displays and wearable computers. Current research into high-speed, flexible electronic substrates uses plastics for the flexible substrate, but these plastics typically have drawbacks, such as high thermal expansion coefficients. Transparent films made from cellulose nanofibrils (CNFs) have low thermal expansion and therefore the potential to serve as substrates for flexible electronics. Initial results show that cellulosic nanomaterials are promising candidates for electronic substrates, and research into the characterization of these substrates and their interactions with electronic devices is ongoing [1].

Keywords: nanofibrils; composites; flexible electronics

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 2,794 kb(s)

Date posted: 09/18/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 65438
Current FPL Scientist associated with this product
Sabo, Ronald C.
Research Materials Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »