Title: Treated and Untreated foam core particleboards with intumescent veneer

Source: Journal of Thermal Analysis and Calorimetry, 2013; 9 p.

Author(s)Dietenberger, Mark A.; Shalbafan, Ali; Welling, Johannes; Boardman, Charles, R..

Publication Year: 2013  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4723-2B

Abstract: The effectiveness of treatments for the surface layer of novel foam core particleboards was evaluated by means of Cone calorimeter tests, Foam cote particleboards with variations of surface layer treatment, adhesives, and surface layer thicknesses under similar processing conditions were used to produce the test specimen for the Cone calorimeter tests. Ignitability, heat release rate profile, peak of heat release rate, total heat released, effective heat of combustion, mass loss rate, gaseous emissions, and specific extinction area were measured using the cone irradiance of 50 kW m-2. Additional analysis of this data provided fuel composition information that could reveal the pyrolysis events of the composite boards. Thermocouples at various depths were used to provide further verification of pyrolysis events. The unprotected foam core panels generally had much higher heat release rates, somewhat higher heat of combustion and much higher smoke production due to the polymeric foam component of tested panels, whereas time to ignition and total heat release were not pronounced from the veneer treated boards. Adding the commercial fire retardant veneer to the face particleboard provided a dramatic improvement to the measured flammability properties. It worked sufficiently well with a 3 mm thick surface layer to improve the predicted flame spread rating of the foam core particleboards.

Keywords: Foam core particleboard, cone calorimeter, sandwich, FRTveneer, Polystyrene foam

Publication Review Process: Formally Refereed

File size: 328 kb(s)

Date posted: 09/06/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 65059
Current FPL Scientist associated with this product
Dietenberger, Mark A.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »