Title: Impact of industrial source on the chemical composition of loblolly pine

Source: Forest Products Journal 62(7/8):516-519

Author(s)Eberhardt, Thomas L.

Publication Year: 2012  View PDF »

Category: Journal Articles

Abstract: The chemical compositions of loblolly pine (Pinus taeda L.) bark samples from two industrial sources were determined for whole bark as well as the inner and outer bark components. Differences in extractive contents of the whole bark samples were primarily attributed to the different debarking methods which afforded different proportions of inner and outer bark. Treatment of the extractive-free bark samples with 1 percent NaOH to remove interfering phenolic compounds impacted the lignin contents determined by the Klason method, but not those determined by the acetyl bromide method. Upon determining the proportions of inner and outer bark, the data provided here can be used to estimate the chemical compositions of other southern yellow pine bark resources.

Publication Review Process: Formally Refereed

File size: 131 kb(s)

Date posted: 08/22/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 64904

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »