Title: Biorefinery opportunities for the forest products industries

Source: In: Van Sambeek, J.W.; Jackson, Elizabeth A.; Coggeshall, Mark V.; Thomas, Andrew L.; Michler, Charles H. eds. 2013. Managing fine hardwoods after a half century of research: Proceedings of the Seventh Walnut Council Research Symposium; 2011 August 1-3; Madison, WI. Gen. Tech. Rep. NRS-P-115. Newtown Square, PA; U.S. Department of Agriculture, Forest Service, Northern Research Station: 15.

Author(s)Rudie, Alan W.

Publication Year: 2013  View PDF »

Category: Not Classified
Associated Research Project(s):   FPL-4709-1B

Abstract: Wood residues offer biorefinery opportunities for new products in our industries including fuel and chemicals. But industry must have two capabilities to succeed with biorefineries. Most forest products companies already have the first capability: knowing where the resource is, how to get it, and how much it will cost. They will need to integrate the acquisition of woody residues for making new products while minimizing competition for valuable timber suitable for dimension lumber and other traditional products.

Keywords: Juglans; plantation culture; nut production

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 301 kb(s)

Date posted: 06/27/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 64293
Current FPL Scientist associated with this product
Rudie, Alan W.
Supervisory Research Chemist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »