Title: Evaluation of the High-Heel Roof-to-Wall Connection with Extended OSB Wall Sheathing

Source: USDA Forest Service, Forest Products Laboratory, General Technical Report, FPL-GTR-222, 2013; 15 p.

Author(s)DeRenzis, Andrew; Kochkin, Vladimir; Wang, Xiping

Publication Year: 2013  View PDF »

Category: General Technical Reports
Associated Research Project(s):   FPL-4714-1B

Abstract: A recently completed testing project conducted to evaluate optimized structural roof-to-wall attachment solutions demonstrated the effectiveness of wood structural panels in restraining high-heel trusses against rotation. This study was designed to further evaluate the performance of OSB wall sheathing panels extended over the high-heel truss in resisting combined uplift and shear forces. Five full-size roof–wall assemblies were constructed with extended OSB wall sheathing and each was tested under a different loading combination. Our test results indicate that using extended wood structural panel wall sheathing as the primary connection element at the roof-to-wall interface of energy trusses can provide a continuous load path in both the shear and uplift directions and can be considered a viable option for residential construction in most areas of the country.

Keywords: Lateral performance; high-heel truss; OSB wall sheathing; roof system; roof-to-wall connection

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 1,403 kb(s)

Date posted: 05/29/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 64005
Current FPL Scientist associated with this product
Wang, Xiping
Research Forest Products Technologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »