Title: Fire performances of foam core particleboards continuously produced in a one-step process

Source: Eur. J. Wood Prod. (2013) Volume 71: pp. 49-59. 2013.

Author(s)Shalbafan, Ali; Dietenberger, Mark A.; Welling, Johannes

Publication Year: 2013  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4723-2B

Abstract: For further progress of novel foam core particleboards, their fire performance was examined with cone calorimetry tests (ASTM E 1354-11a). Specimens with varying surface layer thicknesses, foam densities (polystyrene foam), and processing temperatures were tested. Using the initially recommended cone irradiance of 35 kW/m2, different flammability parameters were measured. In comparison to particleboards, the foam core panels generally had much higher heat release rates, somewhat higher heat of combustion and much higher smoke production due to the EPS-foam component of tested panels. The time to ignition and total heat release did not vary significantly among the samples, although certain trends could be explained. The effects of variations in specimen foam densities and processing temperatures on the flammability parameters were not very significant. However, the flammability properties improved towards that of the reference particleboard as the surface layer thickness increased from 3 to 5 mm.

Keywords: Foams; Layered Structures; Wood Composite

Publication Review Process: Formally Refereed

File size: 895 kb(s)

Date posted: 01/10/2013

This publication is also viewable on Treesearch:  view
RITS Product ID: 63034
Current FPL Scientist associated with this product
Dietenberger, Mark A.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »