Title: Comparative genomics of Ceriporiopsis subvermispora and Phanerochaete chrysosporium provide insight into selective ligninolysis

Source: PNAS , April 3, 2012, volume 109, number 14;2012

Author(s)Fernandez-Fueyo, Elena; Ruiz-Dueñas, Francisco J.; Ferreira, Patricia; Floudas, Dimitrios; Hibbett, David S.; Canessa, Paulo; Larrondo, Luis F.; James, Tim Y.; Seelenfreund, Daniela; Lobos, Sergio; Polanco, Rubén; Tello, Mario; Honda, Yoichi; Watanabe, Takahito; Watanabe, Takashi; Ryu, Jae San; Kubicek, Christian P.; Schmoll, Monika; Gaskell, Jill; Hammel, Kenneth E.; St. John, Franz J.; Wymelenberg, Amber Vanden; Sabat, Grzegorz; BonDurant, Sandra Splinter; Syed, Khajamohiddin; Yadav, Jagjit S.; Dodapaneni, Harshavardhan; Subramanian, Venkataramanan; Lavin, José L.; Oguiza, José A.; Perez, Gumer; Pisabarro, Antonio G.; Ramirez, Lucia; Santoyo, Francisco; Master, Emma; Coutinho, Pedro M.; Henrissat, Bernard; Lombard, Vincent; Magnuson, Jon Karl; Kües, Ursula; Hori, Chiaki; Igarashi, Kiyohiko; Samejima, Masahiro; Held, Benjamin W.; Barry, Kerrie W.; LaButti, Kurt M.; Lapidus, Alla; Lindquist, Erika A.; Lucas, Susan M.; Riley, Robert; Salamov, Asaf A.; Hoffmeister, Dirk; Schwenk, Daniel; Hadar, Yitzhak; Yarden, Oded; de Vries, Ronald P.; Wiebenga, Ad; Stenlid, Jan; Eastwood, Daniel; Grigoriev, Igor V.; Berka, Randy M.; Blanchette, Robert A.; Kersten, Phil; Martinez, Angel T.; Vicuna, Rafael; Cullen, Daniel

Publication Year: 2012  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4712-4A

Abstract: Efficient lignin depolymerization is unique to the wood decay basidiomycetes, collectively referred to as white rot fungi. Phanerochaete chrysosporium simultaneously degrades lignin and cellulose, whereas the closely related species, Ceriporiopsis subvermispora, also depolymerizes lignin but may do so with relatively little cellulose degradation. To investigate the basis for selective ligninolysis, we conducted comparative genome analysis of C. subvermispora and P. chrysosporium. Genes encoding manganese peroxidase numbered 13 and five in C. subvermispora and P. chrysosporium, respectively. In addition, the C. subvermispora genome contains at least seven genes predicted to encode laccases, whereas the P. chrysosporium genome contains none. We also observed expansion of the number of C. subvermispora desaturase-encoding genes putatively involved in lipid metabolism. Microarray-based transcriptome analysis showed substantial upregulation of several desaturase and MnP genes in wood-containing medium. MS identified MnP proteins in C. subvermispora culture filtrates, but none in P. chrysosporium cultures. These results support the importance of MnP and a lignin degradation mechanism whereby cleavage of the dominant nonphenolic structures is mediated by lipid peroxidation products. Two C. subvermispora genes were predicted to encode peroxidases structurally similar to P. chrysosporium lignin peroxidase and, following heterologous expression in Escherichia coli, the enzymes were shown to oxidize high redox potential substrates, but not Mn2+. Apart from oxidative lignin degradation, we also examined cellulolytic and hemicellulolytic systems in both fungi. In summary, the C. subvermispora genetic inventory and expression patterns exhibit increased oxidoreductase potential and diminished cellulolytic capability relative to P. chrysosporium.

Publication Review Process: Formally Refereed

File size: 441 kb(s)

Date posted: 09/18/2012

This publication is also viewable on Treesearch:  view
RITS Product ID: 61480
Current FPL Scientists associated with this product (listed alphabetically)
Cullen, Daniel
Research Microbiologist
Hammel, Kenneth E.
Research Chemist
St. Johns, Franz
Research Microbiologist

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »