Title: A Systematic Approach to the Study of Accelerated weathering of Building Joint Sealants

Source: Journal of ASTM International, Volume 9, Number 5; 2012

Author(s)White, Christopher C.; Hunston, Donald L.; Tan, Kar Tean; Filliben, James J.; Pintar, Adam L.; Schueneman, Greg

Publication Year: 2012  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4707-1A

Abstract: An accurate service life prediction model is needed for building joint sealants in order to greatly reduce the time to market of a new product and reduce the risk of introducing a poorly performing product into the marketplace. A stepping stone to the success of this effort is the precise control of environmental variables in a laboratory accelerated test apparatus in order to produce reliable weathering data that can be used to generate a predictive model. This contribution reports a systematic study, using a novel laboratory test apparatus, investigating the individual and synergistic impacts of four environmental factors (cyclic movement, temperature, relative humidity, and ultraviolet radiation) on the durability of a sealant system. The apparatus used is unique because it not only allows the precise control of environmental factors but also permits in situ characterization tests so that the specimens need not be removed from the apparatus chamber. Graphical and quantitative statistical approaches have been used to analyze the data. The study shows that the critical role of each individual factor, as well as synergism among the different factors, can be readily quantified, and modes of degradation possibly can be identified.

Keywords: Sealant; Service Life Prediction; model; construction; modulus; SPHERE; Statistics

Publication Review Process: Formally Refereed

File size: 749 kb(s)

Date posted: 09/18/2012

This publication is also viewable on Treesearch:  view
RITS Product ID: 61437
Current FPL Scientist associated with this product
Schueneman, Gregory
Supervisory Research Materials Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »