Title: Build Green: Wood Can Last for Centuries

Source: Forest Service, Forest Products Laboratory, General Technical Report, FPL-GTR-215, 2012: 27 p.

Author(s)Clausen, Carol A.; Glass, Samuel V.

Publication Year: 2012  View PDF »

Category: General Technical Reports
Associated Research Project(s):   FPL-4723-4

Abstract: This report updates and revises information from the 1976 Forest Service publication by Rodney C. DeGroot, “Your Wood Can Last for Centuries.” It explains why wood decays, alerts the homeowner to conditions that can result in decay in buildings, and describes measures to prevent moisture-related damage to wood.

Keywords: moisture; decay

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 3,382 kb(s)

Date posted: 09/04/2012

This publication is also viewable on Treesearch:  view
RITS Product ID: 61119
Current FPL Scientists associated with this product (listed alphabetically)
Clausen, Carol A.
Supervisory Research Microbiologist
Glass, Samuel V.
Research Physical Scientist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »