Title: A brief review of machine vision in the context of automated wood identification systems

Source: IAWA journal. Vol. 32, no. 2 (2011): p. 233-250.

Author(s)Hermanson, John C.; Wiedenhoeft, Alex C.

Publication Year: 2011  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4714-1A

Abstract: The need for accurate and rapid field identification of wood to combat illegal logging around the world is outpacing the ability to train personnel to perform this task. Despite increased interest in non-anatomical (DNA, spectroscopic, chemical) methods for wood identification, anatomical characteristics are the least labile data that can be extracted from solid wood products, independent of wood processing (sawing, drying, microbial attack). Wood identification using anatomical characteristics is thus still a viable approach to the wood identification problem, and automating the process of identification is an attractive and plausible solution. The undisputed increase of computer power and image acquisition capabilities, along with the decrease of associated costs, suggests that it is time to move toward non-human based automated wood identification systems and methods. This article briefly reviews the foundations of image acquisition and processing in machine vision systems and overviews how machine vision can be applied to wood identification.

Keywords: Machine vision; wood identification; illegal logging; endangered species; pattern recognition; wood anatomy; image analysis; endangered plants; computer vision; image processing; automatic machinery; wood inspection; logging; law enforcement; optical equipment; optical instruments

Publication Review Process: Formally Refereed

File size: 1,377 kb(s)

Date posted: 09/14/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 39428
Current FPL Scientists associated with this product (listed alphabetically)
Hermanson, John C.
Research General Engineer
Wiedenhoeft, Alex C.
Research Botanist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »