Title: Chapter 5:Drying and heat sterilization of maple lumber for structural uses

Source: Undervalued hardwoods for engineered materials and components. Madison, WI : Forest Products Society ; Marquette, MI : Northern Initiative, [c2005]: Pages 51-63.

Author(s)Simpson, William T.; Wang, Xiping

Publication Year: 2005  View PDF »

Category: Book Chapter

Abstract: Traditional hardwood lumber drying processes were developed for appearance-type products such as furniture, cabinetry, and millwork. This means that air-drying practices were managed to minimize the chemical and fungal stains that occur in white woods such as maple, as well as surface checking that is common in some species. It also means that the kiln schedules which were developed are conservative, slow, and designed to virtually eliminate even minor drying defects such as small surface checks or discolorations. In structural products, surface checks and discoloration do not detract from utility. They are not considered defects in softwood structural lumber grading rules. Therefore, for structural lumber, air-drying and pre-drying practices can be relaxed and kiln schedules can be more severe, faster, and more efficient than traditional hardwood schedules.

Keywords: Hardwoods, heat treatment, drying, lumber, maple, pest control, sterilization, wood moisture, heating time, moisture content, drying schedules, air drying, kiln drying, heat sterilization

File size: 198 kb(s)

Date posted: 12/22/2008

This publication is also viewable on Treesearch:  view
RITS Product ID: 29304
Current FPL Scientist associated with this product
Wang, Xiping
Research Forest Products Technologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »