Title: Antioxidant activity of extracts from the wood and bark of Port OrFord cedar

Source: J. Wood. Sci., Vol. 53: 147-152

Author(s)Gao, Heng; Shupe, Todd F.; Eberhardt, Thomas L.; Hse, Chung Y.

Publication Year: 2007  View PDF »

Category: Not Classified

Abstract: Heartwood, sapwood, and inner and outer bark of Port Orford cedar were extracted with methanol, and the extracts evaluated for antioxidant activity. The total phenol content (TPC) of the extracts was determined by the Folin-Ciocalteu method and expressed as gallic acid equivalent (GAE). Butylated hydroxytoluene was used as a positive control in the free-radical-scavenging activity tests and ethylenediaminetetraacetic acid dihydrate disodium salt served as a positive control in the metal-chelating activity assay. All wood extracts showed significant freeradical-scavenging activity. In the radical-scavenging assay of 2,2-azino-bis (3-ethylbenzothiazoline-6-sulfonic acid) diammonium salt (the ABTS assay), the inner bark extracts exhibited the strongest free-radical-scavenging activity. The 50% inhibitory concentrations (IC50) in the radical-scavenging assay against 1,l-diphenyl-2-picrylhydrazyl hydrate radical (DPPH) of the heartwood, sapwood, and inner and outer bark extracts were 64.77, 29.03, 10.31, 19.87,μgml-1, respectively. In the metal-chelating activity system, the sapwood extract demonstrated significant activity. The greatest TPC, 537.5 mg GAE/g dry extract, was detected in the inner bark. The lowest TPC of 136.9mg GAE/g dry extract was observed in the heartwood dry extract. The results indicate that the antioxidant activities of the extracts are in accordance with the amounts of phenolics present; the inner and outer barks of Port Orford cedar are rich in phenolics and may provide good sources of antioxidants.

Keywords: Free radical scavenger, methanol extracts, Port Orford cedar, total phenol content

File size: 514 kb(s)

Date posted: 10/18/2007

This publication is also viewable on Treesearch:  view
RITS Product ID: 25199

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »