Title: Chinese tallow tree (Sapium sebiferum) utilization: characterization of extractives and cell-wall chemistry

Source: Wood and Fiber Science, Vol. 39(2): 319-324

Author(s)Eberhardt, Thomasl L.; Li, Xiaobo; Shupe, Todd F.; Hse, Chung Y.

Publication Year: 2007  View PDF »

Category: Journal Articles

Abstract: Wood, bark, and the wax-coated seeds from Chinese tallow tree (Sapium sebiferum (L.) Roxb. syn. Triadica sebifera (L.) Small), an invasive tree species in the southeastern United States, were subjected to extractions and degradative chemical analyses in an effort to better understand the mechanism(s) by which this tree species aggressively competes against native vegetation, and also to facilitate utilization efforts. Analysis of the wood extractives by FTIR spectroscopy showed functionalities analogous to those in hydrolyzable tannins, which appeared to be abundant in the bark; as expected, the seeds had a high wax/oil content (43.1%). Compared to other fast-growing hardwoods, the holocellulose content for the Chinese tallow tree wood was somewhat higher (83.3%). The alpha-cellulose (48.3%) and Klason lignin (20.3%) contents were found to be similar to those for most native North American hardwoods. Results suggest that Chinese tallow tree wood utilization along with commercial wood species should not present any significant processing problems related to the extractives or cell-wall chemistry.

Keywords: Cellulose; chinese tallow tree; extractives; klason lignin; utilization

File size: 74 kb(s)

Date posted: 08/22/2007

This publication is also viewable on Treesearch:  view
RITS Product ID: 24776

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »