Title: Mechanical and physical properties of composite panels manufactured from Chinese tallow tree furnish

Source: Forest Products Journal, Vol. 56(6): 64-67

Author(s)Shupe, Todd F.; Groom, Leslie H.; Eberhardt, Thomas L.; Rials, Timothy G.; Hse, Chung Y.; Pesacreta, Thomas

Publication Year: 2006  View PDF »

Category: Journal Articles

Abstract: Chinese tallow tree is a noxious, invasive plant in the southeastern United States. It is generally considered a nuisance and has no current commercial use. The objective of this research was to determine the technical feasibility of using the stem wood of this species for particleboard, fiberboard, and structural flakeboard. Due to its rapid growth, Chinese tallow tree could be a leading raw material for bio-based composite panels. This preliminary study indicated that Chinese tallow tree can be successfully used for all three composite panel types to produce panels meeting various American National Standards Institute grades based modulus of rupture, modulus of elasticity, and internal bond.

Keywords: fiberboard; invasive species; particleboard; stiffness; strength; utilization

File size: 107 kb(s)

Date posted: 07/10/2006

This publication is also viewable on Treesearch:  view
RITS Product ID: 19936

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »