Title: Ultraviolet weathering of HDPE/wood-flour composites coextruded with a clear HDPE cap layer

Source: Polymer Degradation and Stability, 96 (2011) 97-106. doi:10.1016/j.polymdegradstab.2010.10.003; 2011

Author(s)Matuana, Laurent M.; Jin, Shan; Stark, Nicole M.

Publication Year: 2011  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-2A

Abstract: This study examined the effect coextruding a clear HDPE cap layer onto HDPE/wood-flour composites has on the discoloration of coextruded composites exposed to accelerated UV tests. Chroma meter, FTIRATR, XPS, SEM, and UV vis measurements accounted for the analysis of discoloration, functional groups, and degree of oxidation of both uncapped (control) and coextruded composites before and after UV exposures. Two separate discoloration characteristics occurred in the discoloration of composites. For uncapped WPCs (control), chemical changes due to photooxidation resulted in darkening followed by physical changes, including loss of colored wood components from the surface, as well as increased roughness on the surface, which led to lightening of WPCs. By contrast, because a hydrophobic cap layer prevented the loss of colored components from the surface, coextruding a clear hydrophobic HDPE cap layer over WPCs significantly decreased the discoloration during the weathering process. Photooxidation of wood components at the interface accounted for the discoloration of coextruded WPCs before the failure of cap layer. Moreover, as the cap layer absorbed a specified amount of UV light and reduced oxygen available to interface, it decreased the photooxidation rate at the interface compared to that at the WPCs surface.

Keywords: Wood-plastic composites, polyethylene, composite materials, deterioration, weathering, accelerated life testing, wood flour, extrusion process, injection molding of plastics, color fading, ultraviolet radiation, stabilizing agents, light absorption, plastics, extrusion, oxidation, Fourier transform infrared spectroscopy, surface roughness, X-ray photoelectron spectroscopy, HDPE, high density polyethylene, discoloration, wood-plastic materials, accelerated testing, photostabilizers, durability, surface properties, ultraviolet absorber, light absorption, coextrusion, FTIR, XPS

Publication Review Process: Formally Refereed

File size: 1 kb(s)

Date posted: 11/08/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 40132
Current FPL Scientist associated with this product
Stark, Nicole M.
Research Chemical Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »